Upatikanaji: | |
---|---|
Kiasi: | |
Vipengee | Nguvu ya juu, upinzani wa kukandamiza |
Maombi | Chakula, vifaa vya hospitali, maelezo mafupi |
Kazi | Mbinu | Sehemu | Thamani |
ISO 1133-1 | g/10min | 0.35 | |
Uzani (23 ° C) | ISO 1183-2 | g/cm^3 | 0.956 |
Nguvu ya mavuno ya tensile | ISO 527-2 | MPA | 27 |
Mazao ya kuzaa | ISO 527-2 | % | 9 |
Nguvu ya kuvunja nguvu | ISO 527-2 | MPA | 10 |
Elongation wakati wa mapumziko | ISO 527-2 | % | 530 |
Modulus ya elastic | ISO 527-2 | MPA | 1190 |
Modulus ya kubadilika | ISO 178 | MPA | 1310 |
IZOD Athari za Athari (23 ° C) | ISO 180 | KJ/M^2 | 11 |
Hatua ya kuyeyuka | ISO 11357-3 | ℃ | 134 |
Joto la kunyoa la Vicat, A/50 | ISO 306 | ℃ | 129 |
Mkazo wa Mazingira Upinzani, F50 | ASTM D1693 | Masaa | 14 |
![]() | ![]() |
![]() | ![]() | ![]() |
Vipengee | Nguvu ya juu, upinzani wa kukandamiza |
Maombi | Chakula, vifaa vya hospitali, maelezo mafupi |
Kazi | Mbinu | Sehemu | Thamani |
ISO 1133-1 | g/10min | 0.35 | |
Uzani (23 ° C) | ISO 1183-2 | g/cm^3 | 0.956 |
Nguvu ya mavuno ya tensile | ISO 527-2 | MPA | 27 |
Mazao ya kuzaa | ISO 527-2 | % | 9 |
Nguvu ya kuvunja nguvu | ISO 527-2 | MPA | 10 |
Elongation wakati wa mapumziko | ISO 527-2 | % | 530 |
Modulus ya elastic | ISO 527-2 | MPA | 1190 |
Modulus ya kubadilika | ISO 178 | MPA | 1310 |
IZOD Athari za Athari (23 ° C) | ISO 180 | KJ/M^2 | 11 |
Hatua ya kuyeyuka | ISO 11357-3 | ℃ | 134 |
Joto la kunyoa la Vicat, A/50 | ISO 306 | ℃ | 129 |
Mkazo wa Mazingira Upinzani, F50 | ASTM D1693 | Masaa | 14 |
![]() | ![]() |
![]() | ![]() | ![]() |