PE100 | 10 MPa |
Maombi | Tube ya PE |
Bidhaa ya uchambuzi | Faharisi ya ubora | Matokeo ya mtihani | Njia ya mtihani |
Kuonekana kwa granule (granule ya rangi), PC/kg | ≤10 | 0 | SH/T 1541-2006 |
Kiwango cha mtiririko wa molekuli (5.00kg), g/10min | 0.29 ± 0.06 | 0.29 | Q/SY DS 0507 |
Mafadhaiko ya mavuno ya tensile, MPA | ≥20.0 | 22.4 | Q/SY DS 0501 |
Mafadhaiko ya kuvunja,% | ≥350 | 743 | Q/SY DS 0501 |
Nguvu ya athari ya charpy, KJ/M^2 | ≥21.0 | 32 | Q/SY DS 0503 |
Uzani, kilo/m^3 | 949 ± 2 | 949.3 | ISO 1183-2 |
Granule kubwa na ndogo | ≤10 | 0 | SH/T 1541-2006 |
![]() | ![]() | ![]() | ![]() |
![]() | ![]() | ![]() |
PE100 | 10 MPa |
Maombi | Tube ya PE |
Bidhaa ya uchambuzi | Faharisi ya ubora | Matokeo ya mtihani | Njia ya mtihani |
Kuonekana kwa granule (granule ya rangi), PC/kg | ≤10 | 0 | SH/T 1541-2006 |
Kiwango cha mtiririko wa molekuli (5.00kg), g/10min | 0.29 ± 0.06 | 0.29 | Q/SY DS 0507 |
Mafadhaiko ya mavuno ya tensile, MPA | ≥20.0 | 22.4 | Q/SY DS 0501 |
Mafadhaiko ya kuvunja,% | ≥350 | 743 | Q/SY DS 0501 |
Nguvu ya athari ya charpy, KJ/M^2 | ≥21.0 | 32 | Q/SY DS 0503 |
Uzani, kilo/m^3 | 949 ± 2 | 949.3 | ISO 1183-2 |
Granule kubwa na ndogo | ≤10 | 0 | SH/T 1541-2006 |
![]() | ![]() | ![]() | ![]() |
![]() | ![]() | ![]() |