| Permohonan | tiub |

Item ujian, unit |
Produk unggul |
Keputusan ujian |
|
Kelikatan mL/g |
127-135 |
133 |
|
Ketumpatan ketara g/mL |
≥ | 0.45 |
0.50 |
Bahan meruap (termasuk air) pecahan jisim % |
≤ | 0.30 |
0.28 |
Sisa ayak 250μn, lubang ayak % |
≤ | 1.6 |
1.5 |
Sisa ayak 63μn, lubang ayak % |
≥ | 97 |
99 |
PC mata ikan/400cm^2 |
≤ | 20 |
17 |
100g resin plasticizer penyerapan,g |
≥ | 26 |
- |
Keputihan(160℃,10min) % |
≥ | 78 |
84 |
| Kekotoran, pcs | ≤ | 16 | 16 |
| Kandungan Monomer Polietilena Baki,μg/g | ≤ | 5.0 | 2 |
| Kekonduksian benzena air,μs/(cm*g) | ≤ | 5.0 | 2 |

|
|
|


![]() |
![]() |
![]() |