Kuonekana | Poda nyeupe | Poda nyeupe |
Kiwango cha wastani cha upolimishaji p | 981 ~ 1080 | 1010 |
Idadi ya chembe za uchafu, PC | ≤ 16 | 4 |
Jambo tete (pamoja na maji),% | ≤ 0.30 | 0.12 |
Wiani dhahiri, g/ml | 0.51 ~ 0.57 | 0.51 |
Mabaki ya ungo 250μm, % | ≤ 1.6 | 0.7 |
Idadi ya 'Macho ya samaki ', PCS/400cm^2 | ≤ 20 | 4 |
Uingizaji wa plastiki, g/100g | ≥ 20 | 22 |
Weupe (160 ℃, 10min),% | ≥.78 | 81 |
Mabaki ya nitrojeni vinyl monomer, μg/g | ≤ 1 | 0.1 |
Wakati wa mtiririko wa kavu, s/400cm^3 | 2.0 ~ 6.0 | 3.4 |
![]() | ![]() |
![]() | ![]() | ![]() |
Vipengee | Kiwango, upinzani wa joto |
Maombi | Tubing |
Vitu vya mtihani | Kielelezo | Matokeo ya mtihani |
Kuonekana | Poda nyeupe | Poda nyeupe |
Kiwango cha wastani cha upolimishaji p | 981 ~ 1080 | 1010 |
Idadi ya chembe za uchafu, PC | ≤ 16 | 4 |
Jambo tete (pamoja na maji),% | ≤ 0.30 | 0.12 |
Wiani dhahiri, g/ml | 0.51 ~ 0.57 | 0.51 |
Mabaki ya ungo 250μm, % | ≤ 1.6 | 0.7 |
Idadi ya 'Macho ya samaki ', PCS/400cm^2 | ≤ 20 | 4 |
Uingizaji wa plastiki, g/100g | ≥ 20 | 22 |
Weupe (160 ℃, 10min),% | ≥.78 | 81 |
Mabaki ya nitrojeni vinyl monomer, μg/g | ≤ 1 | 0.1 |
Wakati wa mtiririko wa kavu, s/400cm^3 | 2.0 ~ 6.0 | 3.4 |
![]() | ![]() |
![]() | ![]() | ![]() |