| Ciri-ciri | keliatan tinggi, rintangan penuaan |
| Permohonan | bekas, filem pertanian, filem susut, pembungkusan, beg plastik |

Item Analisis |
Produk Cemerlang |
Produk Berkelayakan |
Keputusan ujian |
Kaedah eksperimen |
Zarah Hitam |
0 |
0 |
0 |
SH/T 1541-2006 |
Zarah Warna |
≤10 | ≤6 |
0 |
SH/T 1541-2006 |
Zarah Besar dan Kecil,g/kg |
laporan | laporan |
0 |
SH/T 1541-2006 |
Zarah Ekor |
≤20 | ≤40 |
0 |
SH/T 1541-2006 |
Flok,g/kg |
laporan | laporan |
0 |
SH/T 1541-2006 |
Ketumpatan,g/cm^3 |
0.9225±0.0020 | 0.9225±0.0030 |
0.9213 |
GB/T 1033.2-2010 |
MFR,g/10min |
2.0±0.2 | 2.0±0.3 |
2 |
GB/T 3682-2000 |
Terikan Tegangan Nominal pada Pecah,% |
≥70 | ≥70 |
110 |
GB/T 1040.2-2006 |
Kekuatan Tegangan pada Pecah,Mpa |
≥11 | ≥9.5 |
11.5 |
GB/T 1040.2-2006 |
Jerebu,% |
≤9.0 | ≤9.0 |
7.7 |
GB/T 2410-2008 |
Mata ikan, 0.3mm-2.0mm /1200cm^2 |
≤15 | ≤30 |
11 |
GB/T 11115-2009 |
belang |
≤20 | ≤20 |
0 |
GB/T 11115-2009 |

![]() |
![]() |
![]() |
![]() |


![]() |
![]() |
![]() |